Products & Solutions

REXALPHAR series RA FS 059 S

  • Achieves fine line and fine pattern printing with excellent linearity and reproducibility
  • Good adhesion to substrates such as ITO deposited film and PET film
  • Stable print quality can be obtained during continuous printing, and the paste can be reused using a special solvent.
Functions Fine printability, high conductivity
Application example RFID antenna, touch panel, circuit formation, IC card, electronic paper, heater
Applicable base material PET, ITO substrates, paper, glass, etc.
Representative characteristics
Characteristics table (reference value)
Product name RA FS 059 S Remarks
hardening type heat curing Recommended: 135℃ x 30 minutes
Appearance ocher color with silver luster, paste-like
Viscosity (Pa・s@25℃) 130 E-type viscometer・5rpm
Volume resistivity (Ω・cm) 4×10-5 Drying at 135℃ x 30 minutes
Printing method flat screen

*The above values are representative values and are not guaranteed values.

Example of continuous thin line printing

細線連続印刷例

*Conditions Plate: 500 mesh Wire diameter: 18um Emulsion thickness: 7um Gauze thickness: 30um

How to use ink and precautions
  • Please stir the silver paste thoroughly before use.
  • Please store refrigerated (below 0℃ to 10℃).
  • If the paste viscosity is high and printing is difficult, add a solvent ofbutyl diglycol acetate or ethyldiglycolacetate within 1.0%. Please note that excessive addition will impair print reproducibility such as deterioration of linearity and thickening of lines.
  • We recommend using a ketone solvent to clean the plate. Cleaned with our product "S705 Solvent 2KC (Cyclohexanone)" and wiped with "VC102 Solvent C (MEK)".
  • If the paste viscosity increases after printing compared to the paste viscosity immediately after opening (recommended viscosity measurement conditions: E-type viscometer, rotor No. 7, 5 rpm, 25℃), adjust the viscosity so that it becomes the same as after opening. dilute with butyl diglycol acetate solvent.
Requests for use
  1. This material is an example of our experimental data and cannot be guaranteed as the properties obtained will vary depending on printing/processing conditions, base materials, etc. Before using the product, please carefully check its intended use.
  2. Before handling this product, be sure to read the "Product Safety Data Sheet" and handle with care.
  3. If you are exporting this product overseas, please be sure to check with us.

Inquiries

TOYO INK CO., LTD. Marketing Headquarters New Business Development Department

TOYO INK CO., LTD.